Link to full record for micrograph 63 Micrograph 63 : Fe, C 3.6, Si 2.1 (wt%), hypereutectic grey cast iron
System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 64 Micrograph 64 : Fe, C 3.6, Si 2.1, Mg 0.07 (wt%), spheroidal graphite
System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1, Mg 0.07 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 65 Micrograph 65 : Fe, C 3.6, Si 2.1, Mg 0.07 (wt%), spheroidal graphite
System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1, Mg 0.07 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 66 Micrograph 66 : Hypoeutectic white cast iron
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
400 μm
Link to full record for micrograph 67 Micrograph 67 : Hypoeutectic white cast iron
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
80 μm
Link to full record for micrograph 68 Micrograph 68 : Grey cast iron core with white cast iron periphery
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
200 μm
Link to full record for micrograph 69 Micrograph 69 : Grey cast iron core with white cast iron periphery
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
40 μm
Link to full record for micrograph 70 Micrograph 70 : Silal
System: Fe-C-X, Composition: Fe, C 3.0, Si 6, Mn 0.7, P 0.3, S 0.1 (wt% typical) (Silal)
Reflected light microscopy
200 μm
Link to full record for micrograph 71 Micrograph 71 : Silal
System: Fe-C-X, Composition: Fe, C 3.0, Si 6, Mn 0.7, P 0.3, S 0.1 (wt% typical) (Silal)
Reflected light microscopy
80 μm
Link to full record for micrograph 72 Micrograph 72 : Ni-hard iron
System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron)
Reflected light microscopy
400 μm