272 micrographs for keyword iron, ordered by micrograph number.


Showing 61 - 70 of 272 micrographs Page 1 .. 4 5 6 7 8 9 10 .. 28 | Previous | Next

Link to full record for micrograph 224 Micrograph 224 : Annealed low carbon steel with carbides
System: Fe-C-X, Composition: Fe, C low (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 225 Micrograph 225 : Normalised steel
System: Fe-C-X, Composition: Fe, C 0.55 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 226 Micrograph 226 : Normalised steel
System: Fe-C-X, Composition: Fe, C 0.55 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 227 Micrograph 227 : Normalised steel
System: Fe-C-X, Composition: Fe, C 0.4 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 228 Micrograph 228 : Normalised steel
System: Fe-C-X, Composition: Fe, C 0.4 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 229 Micrograph 229 : Normalised steel
System: Fe-C-X, Composition: Fe, C 0.5 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 230 Micrograph 230 : Normalised steel
System: Fe-C-X, Composition: Fe, C 0.5 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 231 Micrograph 231 : Normalised steel
System: Fe-C-X, Composition: Fe, C 0.6 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 232 Micrograph 232 : Normalised steel
System: Fe-C-X, Composition: Fe, C 0.6 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 233 Micrograph 233 : Hypoeutectoid steel, normalised at 1100°C
System: Fe-C-X, Composition: Fe, C 0.4 (wt%)
Reflected light microscopy
400 μm