172 micrographs for keyword steel, ordered by micrograph number.
Showing 151 - 160 of 172 micrographs | Page 1 .. 12 13 14 15 16 17 18 | Previous | Next |
![]() |
Micrograph
339
:
Fe, C 1.35 (wt%) steel, quenched System: Fe-C-X, Composition: Fe, C 1.35 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
340
:
Low alloy medium carbon steel, containing Ni, Cr, Mo, annealed System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
341
:
Low alloy medium carbon steel, containing Ni, Cr, Mo, annealed System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
342
:
Medium carbon, low alloy steel System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
343
:
Medium carbon, low alloy steel System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
344
:
Medium carbon, low alloy steel. System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
345
:
Medium carbon, low alloy steel, isothermally transformed System: Fe-C-X, Composition: Fe, C 0.4, Ni 1.3, Cr 0.65, Mo 0.65 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
346
:
Fe, C 1.35 (wt%) steel, hypereutectoid, quenched System: Fe-C-X, Composition: Fe, C 1.35 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
347
:
Fe, C 1.35 (wt%) steel, hypereutectoid, quenched System: Fe-C-X, Composition: Fe, C 1.35 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
348
:
Fe, C 1.35 (wt%) steel, hypereutectoid, quenched System: Fe-C-X, Composition: Fe, C 1.35 (wt%) Reflected light microscopy 400 μm |
Showing 151 - 160 of 172 micrographs | Page 1 .. 12 13 14 15 16 17 18 | Previous | Next |