Link to full record for micrograph 12 Micrograph 12 : Cu 21, Sn 79 (wt%), peritectic transformation
System: Cu-Sn, Composition: Cu 21, Sn 79 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 13 Micrograph 13 : Cu 21, Sn 79 (wt%), peritectic transformation
System: Cu-Sn, Composition: Cu 21, Sn 79 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 437 Micrograph 437 : Cu, Sn 20 (wt%) bronze, exhibiting dendritic solidification
System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 438 Micrograph 438 : Cu, Sn 20 (wt%) bronze, exhibiting dendritic solidification
System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 484 Micrograph 484 : Cu 80, Sn 20 (wt%) bronze, exhibiting dendritic solidification
System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 485 Micrograph 485 : Cu 80, Sn 20 (wt%) bronze, exhibiting dendritic solidification
System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 486 Micrograph 486 : Cu 80, Sn 20 (wt%) bronze, exhibiting dendritic solidification
System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 487 Micrograph 487 : Cu 85, Sn 15 (wt%) bronze, annealed at 650°C
System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 488 Micrograph 488 : Cu 85, Sn 15 (wt%) bronze, annealed at 650°C
System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 489 Micrograph 489 : Cu 85, Sn 15 (wt%) bronze, annealed at 650°C
System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%)
Reflected light microscopy
100 μm