34 micrographs for keyword nickel, ordered by micrograph number.
| Showing 11 - 20 of 34 micrographs | Page 1 2 3 4 | Previous | Next |
![]() |
Micrograph
391
:
Nickel hard cast iron, martensitic System: Fe-C-X, Composition: Fe, C 2.95, Si 0.60, Mn 0.60, Ni 4.00, Cr 1.90 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
392
:
Nickel hard cast iron, martensitic System: Fe-C-X, Composition: Fe, C 2.95, Si 0.60, Mn 0.60, Ni 4.00, Cr 1.90 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
439
:
a b nickel brass containing 2% lead. System: Cu-Zn, Composition: Cu 46, Zn 42, Ni 10, Pb 2 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
440
:
a b nickel brass containing 2% lead. System: Cu-Zn, Composition: Cu 46, Zn 42, Ni 10, Pb 2 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
713
:
IN718 nickel-based superalloy held for 1 minute at 850°C System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al Reflected light microscopy, cross-polarised, with Nomarski filter 20 μm |
![]() |
Micrograph
714
:
IN718 nickel-based superalloy held for 20 minutes at 850°C System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al Reflected light microscopy, cross-polarised, with Nomarski filter 20 μm |
![]() |
Micrograph
715
:
IN718 nickel-based superalloy held for 1 hour at 850°C System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al Reflected light microscopy, cross-polarised, with Nomarski filter 25 μm |
![]() |
Micrograph
716
:
IN718 nickel-based superalloy held for 3 hours at 850°C System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al Reflected light microscopy, cross-polarised, with Nomarski filter 25 μm |
![]() |
Micrograph
717
:
IN718 nickel-based superalloy held for 6 hours at 850°C System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al Reflected light microscopy, cross-polarised, with Nomarski filter 25 μm |
![]() |
Micrograph
718
:
IN718 nickel-based superalloy held for 24 hours at 850°C System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al Reflected light microscopy, cross-polarised, with Nomarski filter 25 μm |