Micrograph
42
:
Zn, cold rolled - mechanical twins System: Zn, Composition: Not specified Reflected light microscopy 80 μm |
![]() |
Micrograph
49
:
Cu 60, Zn 40 (wt%), slow cooling - equiaxed grains System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
50
:
Cu 60, Zn 40 (wt%), slow cooling - equiaxed grains System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
51
:
Cu 60, Zn 40 (wt%), air cooled - Widmanstätten microstructure System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
52
:
Cu 60, Zn 40 (wt%), air cooled - Widmanstätten microstructure System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
53
:
Cu 60, Zn 40 (wt%), quenched and held at 300°C - Widmanstätten microstructure System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Scanning electron microscopy (SEM) 15 μm |
![]() |
Micrograph
75
:
Notched zinc, broken by impact at room temperature System: Zn, Composition: Notched zinc Scanning electron microscopy (SEM) 1 mm |
![]() |
Micrograph
76
:
Notched zinc, broken by impact at room temperature System: Zn, Composition: Notched zinc Scanning electron microscopy (SEM) 160 μm |
![]() |
Micrograph
144
:
Zinc, notched specimen, failed through brittle cleavage fracture. System: Zn, Composition: Not specified Scanning electron microscopy (SEM) 200 μm |
![]() |
Micrograph
145
:
Zinc, notched specimen, failed through brittle cleavage fracture. System: Zn, Composition: Not specified Scanning electron microscopy (SEM) 1 mm |
| Showing 11 - 20 of 80 micrographs | Page 1 2 3 4 5 6 7 8 | Previous | Next |