Keyword
274 micrographs for keyword carbon, ordered by micrograph number.
Showing 201 - 210 of 274 micrographs | Page 1 .. 18 19 20 21 22 23 24 .. 28 | Previous | Next |
Micrograph
379
:
Grey cast iron with significant Si content System: Fe-C-X, Composition: Fe, C 3.52, Si 3.26, Mn 0.47 (wt%) (Grey cast iron) Reflected light microscopy 200 μm |
|
Micrograph
380
:
Grey cast iron with significant Si content System: Fe-C-X, Composition: Fe, C 3.52, Si 3.26, Mn 0.47 (wt%) (Grey cast iron) Reflected light microscopy 100 μm |
|
Micrograph
381
:
Grey cast iron System: Fe-C-X, Composition: Grey cast iron Reflected light microscopy 400 μm |
|
Micrograph
382
:
Grey cast iron System: Fe-C-X, Composition: Grey cast iron Reflected light microscopy 200 μm |
|
Micrograph
383
:
Grey cast iron System: Fe-C-X, Composition: Grey cast iron Reflected light microscopy 100 μm |
|
Micrograph
384
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.3, Mn 4.0 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
385
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.3, Mn 4.0 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
386
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.3, Mn 4.0 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
387
:
Silal System: Fe-C-X, Composition: Fe, C 2.10, Si 5.60, Mn 0.50 (wt%) (Silal) Reflected light microscopy 400 μm |
|
Micrograph
388
:
Silal System: Fe-C-X, Composition: Fe, C 2.10, Si 5.60, Mn 0.50 (wt%) (Silal) Reflected light microscopy 200 μm |
Showing 201 - 210 of 274 micrographs | Page 1 .. 18 19 20 21 22 23 24 .. 28 | Previous | Next |