Dissemination of IT for the Promotion of Materials Science (DoITPoMS)

Keyword

274 micrographs for keyword carbon, ordered by micrograph number.


Showing 221 - 230 of 274 micrographs Page 1 .. 20 21 22 23 24 25 26 .. 28 | Previous | Next

Link to full record for micrograph 402 Micrograph 402 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
100 μm
Link to full record for micrograph 403 Micrograph 403 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
400 μm
Link to full record for micrograph 404 Micrograph 404 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
200 μm
Link to full record for micrograph 405 Micrograph 405 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
100 μm
Link to full record for micrograph 406 Micrograph 406 : Cast iron, containing phosphorus
System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 407 Micrograph 407 : Cast iron, containing phosphorus
System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 408 Micrograph 408 : Cast iron, containing phosphorus
System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 409 Micrograph 409 : Cast iron, containing phosphorus
System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 410 Micrograph 410 : Cast iron, containing phosphorus
System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 411 Micrograph 411 : Cast iron, containing phosphorus
System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%)
Reflected light microscopy
100 μm

Showing 221 - 230 of 274 micrographs Page 1 .. 20 21 22 23 24 25 26 .. 28 | Previous | Next

List all keywords