Keyword
18 micrographs for keyword magnesium, ordered by micrograph number.
Showing 1 - 10 of 18 micrographs | Page 1 2 | Previous | Next |
![]() |
Micrograph
64
:
Fe, C 3.6, Si 2.1, Mg 0.07 (wt%), spheroidal graphite System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1, Mg 0.07 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
65
:
Fe, C 3.6, Si 2.1, Mg 0.07 (wt%), spheroidal graphite System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1, Mg 0.07 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
148
:
Magnesia-chrome refractory brick System: MgO-Cr2O3, Composition: MgO 70, Cr2O3 19, Al2O3 4, Fe2O3 4, CaO 1, SiO2 1 (wt%) Reflected light microscopy 1 mm |
![]() |
Micrograph
149
:
Magnesia-chrome refractory brick System: MgO-Cr2O3, Composition: MgO 70, Cr2O3 19, Al2O3 4, Fe2O3 4, CaO 1, SiO2 1 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
154
:
Macor(TM) Machinable Glass Ceramic System: MAS (MgO-Al2O3-SiO2), Composition: SiO2 47, B2O3 8, Al2O3 17, MgO 14, K2O 9, F 6 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
710
:
Wrought-grade aluminium alloy (Al-Mg-Fe-Si containing < 1wt.% of each solute); refined with TiB2 particles. Deformation of grain structure is due to cutting of sample with scissors. System: Al-Mg-Fe-Si, Composition: Not specified Cross-polarised light microscopy 400 μm |
![]() |
Micrograph
711
:
As-cast wrought-grade aluminium alloy (Al-Mg-Fe-Si containing < 1wt.% of each solute). No addition of grain refinement particles (e.g. TiB2). System: Al-Mg-Fe-Si, Composition: Not specified Cross-polarised light microscopy 1 mm |
![]() |
Micrograph
712
:
As-cast wrought-grade aluminium alloy (Al-Mg-Fe-Si containing < 1wt.% of each solute). Addition of TiB2 particles facilitates the formation of a fine, equiaxed grain structure (grain refinement). System: Al-Mg-Fe-Si, Composition: Not specified Cross-polarised light microscopy 400 μm |
![]() |
Micrograph
730
:
Magnesium alloy System: Mg-Zn, Composition: Mg 94.05, Zn 5.62, Zr 0.19, Ce 0.10, Nd 0.03 (wt%) (RZ5 Alloy) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 200 μm |
![]() |
Micrograph
732
:
Magnesium alloy System: Mg-Zn, Composition: Mg 94.05, Zn 5.62, Zr 0.19, Ce 0.10, Nd 0.03 (wt%) (RZ5 Alloy) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 200 μm |