Micrograph
355
:
Pearlitic malleable cast iron System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 200 μm |
![]() |
Micrograph
356
:
Pearlitic malleable cast iron System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
357
:
Pearlitic malleable cast iron System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
358
:
White cast iron, annealed to precipitate out carbon System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
359
:
White cast iron, annealed to precipitate out carbon System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
360
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
361
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
384
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.3, Mn 4.0 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
385
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.3, Mn 4.0 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
386
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.3, Mn 4.0 (wt%) Reflected light microscopy 200 μm |