Keyword
69 micrographs for keyword cast iron, ordered by micrograph number.
| Showing 21 - 30 of 69 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |
![]() |
Micrograph
393
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 400 μm |
![]() |
Micrograph
394
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 200 μm |
![]() |
Micrograph
395
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 100 μm |
![]() |
Micrograph
396
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 400 μm |
![]() |
Micrograph
397
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy, polarised 400 μm |
![]() |
Micrograph
398
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 200 μm |
![]() |
Micrograph
399
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 100 μm |
![]() |
Micrograph
400
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 400 μm |
![]() |
Micrograph
401
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 100 μm |
![]() |
Micrograph
402
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 100 μm |
| Showing 21 - 30 of 69 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |