3 micrographs for keyword order hardening, ordered by micrograph number.


Link to full record for micrograph 79 Micrograph 79 : Ni-superalloy, fatigue crack propagation
System: Ni-X, Composition: Not specified (Ni-Superalloy)
Scanning electron microscopy (SEM)
150 μm
Link to full record for micrograph 80 Micrograph 80 : Ni-superalloy, fatigue crack propagation
System: Ni-X, Composition: Not specified (Ni-Superalloy)
Scanning electron microscopy (SEM)
80 μm
Link to full record for micrograph 81 Micrograph 81 : Ni-superalloy, fatigue crack propagation
System: Ni-X, Composition: Not specified (Ni-Superalloy)
Scanning electron microscopy (SEM)
30 μm