14 micrographs for keyword twinning, ordered by micrograph number.


Showing 1 - 10 of 14 micrographs Page 1 2 | Previous | Next

Link to full record for micrograph 31 Micrograph 31 : Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 32 Micrograph 32 : Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 33 Micrograph 33 : Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 34 Micrograph 34 : Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 37 Micrograph 37 : Cu 70, Zn 30 (wt%), slow cooling - annealing twins
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 38 Micrograph 38 : Cu 98, Be 2 (wt%), slow cooling - annealing twins
System: Cu-Be, Composition: Cu 98, Be 2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 39 Micrograph 39 : Cu 98, Be 2 (wt%), quenched and aged - annealing twins
System: Cu-Be, Composition: Cu 98, Be 2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 40 Micrograph 40 : Cu 98, Be 2 (wt%), quenched and aged - annealing twins
System: Cu-Be, Composition: Cu 98, Be 2 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 41 Micrograph 41 : Zn, cold rolled - mechanical twins
System: Zn, Composition: Not specified
Reflected light microscopy
400 μm
Link to full record for micrograph 42 Micrograph 42 : Zn, cold rolled - mechanical twins
System: Zn, Composition: Not specified
Reflected light microscopy
80 μm

Showing 1 - 10 of 14 micrographs Page 1 2 | Previous | Next