Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Micrograph 427 and full record
- Micrograph no
- 427
- Brief description
- Cu 70, Zn 30 (wt%), recrystallised - annealing twins
- Keywords
- alloy
, annealing
, annealing twins
, brass
, copper, metal, zinc - Categories
- Metal or alloy
- System
- Cu-Zn
- Composition
- Cu 70, Zn 30 (wt%)
- Standard codes
- Reaction
- Processing
- Cast wrought annealed
- Applications
- Sample preparation
- Ammonium persulphate
- Technique
- Reflected light microscopy
- Length bar
- 400 μm
- Further information
- Annealing causes the alloy to recrystallise and grow. This results in a single a phase containing annealing twins.
- Contributor
- Dr R F Cochrane
- Organisation
- Department of Materials, University of Leeds
- Date
- 04/09/02
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International- Related micrographs
- Micrograph 428: Cu 70, Zn 30 (wt%), recrystallised - annealing twins (200 μm)
- Micrograph 429: Cu 70, Zn 30 (wt%), recrystallised - annealing twins (400 μm)
- Micrograph 430: Cu 70, Zn 30 (wt%), recrystallised - annealing twins (100 μm)
- Micrograph 431: Cu 80, Zn 20 (wt%), recrystallised - annealing twins (400 μm)
- Micrograph 432: Cu 80, Zn 20 (wt%), recrystallised - annealing twins (200 μm)
- Micrograph 433: Cu 90, Zn 10 (wt%), recrystallised - annealing twins (400 μm)
- Micrograph 434: Cu 90, Zn 10 (wt%), recrystallised - annealing twins (200 μm)
View image alone .. in a new window
Help is available on downloading images