Micrograph 842 and full record
- Micrograph no
- 842
- Brief description
- Macrograph of a resistance spot weld made in two plates of 1,5mm thickness. T3 - solution heat treatment, cold working and natural ageing.
- Keywords
- aluminium
, copper - Categories
- Metal or alloy
- System
- Al-Cu
- Composition
- Al, Cu 4.5, Mg 1.5 (wt%)
- Standard codes
- Reaction
- Processing
- Applications
- Typically used in aerospace industry due to excellent mechanical properties.
- Sample preparation
- Polished and etched with Keller's reagent (swabbed for 15-20s) then rinsed with running water and dried with compressed air.
- Technique
- Optical microscope, interferential contrast
- Length bar
- 1 mm
- Further information
- (AA2024-T3 RSW x40 Keller's reagent interferential contrast)
Base material characterised by elongated, plastically deformed grains. Presence of dendritic grains in the weld. The line on the left is the original plates separation line. The two short lines on the right (inside the weld) are solidification cracks.
- Contributor
- J Adamowski
- Organisation
- Department of Production Engineering, Thermoenergetics and Mathematical Models, University of Genoa, Italy
- Date
- 04/07/05
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International
View image alone .. in a new window
Help is available on downloading images