System
18 micrographs for system Smithing slag, ordered by micrograph number.
| Showing 11 - 18 of 18 micrographs | Page 1 2 | Previous | Next |
![]() |
Micrograph
946
:
Carthage, smithing slag phoenician System: Smithing slag, Composition: Not specified Transmitted light microscopy 500 μm |
![]() |
Micrograph
947
:
Wienhagen W Kierspe (Nr. 72), Grabung Willms System: Smithing slag, Composition: Not specified Transmitted light microscopy 500 μm |
![]() |
Micrograph
948
:
Experimental hammerscale, Denig, Kaiserslautern, Germany System: Smithing slag, Composition: Not specified Reflected light microscopy 100 μm |
![]() |
Micrograph
949
:
Carthage, smithing slag, phoenician System: Smithing slag, Composition: Not specified Transmitted light microscopy 100 μm |
![]() |
Micrograph
956
:
Carthage, smithing slag, phoenician System: Smithing slag, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
959
:
Carthage, smithing slag, phoenician System: Smithing slag, Composition: Not specified Transmitted light microscopy 1 mm |
![]() |
Micrograph
970
:
Elisenhof, Juetland, Germany. Medieval smithing slag System: Smithing slag, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
972
:
Smithing slag Carthage, phoenician System: Smithing slag, Composition: Not specified Transmitted light microscopy 200 μm |
| Showing 11 - 18 of 18 micrographs | Page 1 2 | Previous | Next |