331 micrographs for system Fe-C-X, ordered by micrograph number.
Showing 1 - 10 of 331 micrographs | Page 1 2 3 4 5 6 7 .. 34 | Previous | Next |
![]() |
Micrograph
14
:
Fe, C 0.8 (wt%), eutectoid transformation - pearlite (coarse) System: Fe-C-X, Composition: Fe, C 0.8 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
15
:
Fe, C 0.8 (wt%), eutectoid transformation - pearlite (coarse) System: Fe-C-X, Composition: Fe, C 0.8 (wt%) Reflected light microscopy 40 μm |
![]() |
Micrograph
16
:
Fe, C 0.8 (wt%), eutectoid transformation - pearlite (coarse) System: Fe-C-X, Composition: Fe, C 0.8 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
17
:
Fe, C 0.1 (wt%), hypoeutectoid alloy System: Fe-C-X, Composition: Fe, C 0.1 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
18
:
Fe, C 0.1 (wt%), hypoeutectoid alloy System: Fe-C-X, Composition: Fe, C 0.1 (wt%) Reflected light microscopy 40 μm |
![]() |
Micrograph
19
:
Fe, C 0.1 (wt%), hypoeutectoid alloy System: Fe-C-X, Composition: Fe, C 0.1 (wt%) Scanning electron microscopy (SEM) 30 μm |
![]() |
Micrograph
20
:
Fe, C 0.1 (wt%), hypoeutectoid alloy System: Fe-C-X, Composition: Fe, C 0.1 (wt%) Scanning electron microscopy (SEM) 10 μm |
![]() |
Micrograph
21
:
Fe, C 1.0 (wt%), hypereutectoid alloy System: Fe-C-X, Composition: Fe, C 1.0 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
22
:
Fe, C 1.0 (wt%), hypereutectoid alloy System: Fe-C-X, Composition: Fe, C 1.0 (wt%) Reflected light microscopy 40 μm |
![]() |
Micrograph
23
:
Fe, C 1.0 (wt%), hypereutectoid alloy System: Fe-C-X, Composition: Fe, C 1.0 (wt%) Scanning electron microscopy (SEM) 50 μm |