System
6 micrographs for system Zn, ordered by micrograph number.
![]() |
Micrograph
41
:
Zn, cold rolled - mechanical twins System: Zn, Composition: Not specified Reflected light microscopy 400 μm |
![]() |
Micrograph
42
:
Zn, cold rolled - mechanical twins System: Zn, Composition: Not specified Reflected light microscopy 80 μm |
![]() |
Micrograph
75
:
Notched zinc, broken by impact at room temperature System: Zn, Composition: Notched zinc Scanning electron microscopy (SEM) 1 mm |
![]() |
Micrograph
76
:
Notched zinc, broken by impact at room temperature System: Zn, Composition: Notched zinc Scanning electron microscopy (SEM) 160 μm |
![]() |
Micrograph
144
:
Zinc, notched specimen, failed through brittle cleavage fracture. System: Zn, Composition: Not specified Scanning electron microscopy (SEM) 200 μm |
![]() |
Micrograph
145
:
Zinc, notched specimen, failed through brittle cleavage fracture. System: Zn, Composition: Not specified Scanning electron microscopy (SEM) 1 mm |