Micrograph
876
:
Los Millares, Almeria, Spain. Chalcolithic (arsenical)-copper production. System: Zn, Composition: Not specified Reflected light microscopy 100 μm |
![]() |
Micrograph
877
:
Los Millares, Almeria, Spain. Chalcolithic (arsenical)-copper production. System: Zn, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
878
:
Nörten-Hardenberg (Goettingen) Germany. Smithing slag (hallstatt - latène) System: Zn, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
879
:
Nörten-Hardenberg (Goettingen) Germany. Smithing slag System: Zn, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
880
:
Nörten-Hardenberg (Goettingen) Germany. Smithing slag (hallstatt - latène) System: Zn, Composition: Not specified Transmitted light microscopy 200 μm |
![]() |
Micrograph
881
:
Nörten-Hardenberg (Goettingen) Germany. Smithing slag (hallstatt - latène) System: Zn, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
882
:
Nörten-Hardenberg (Goettingen) Germany. Smithing slag (hallstatt - latène) System: Zn, Composition: Not specified Transmitted light microscopy 200 μm |
![]() |
Micrograph
883
:
Hambach forest, Germany. Medieval smithing slag System: Zn, Composition: Not specified Reflected light microscopy 100 μm |
![]() |
Micrograph
884
:
Monte Romero, Huelva district, Spain. Phoenician, preroman silverproduction from complex ores. System: Zn, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
885
:
Monte Romero, Huelva district, Spain. Phoenician, preroman silver production from complex ores. System: Zn, Composition: Not specified Reflected light microscopy 500 μm |