System
5 micrographs for system Polyhydroxybutyrate (PHB), ordered by micrograph number.
![]() |
Micrograph
600
:
Spherulite in poly-3-hydroxy butyrate (PHB) System: Polyhydroxybutyrate (PHB), Composition: Not specified Cross-polarised light microscopy 1 μm |
![]() |
Micrograph
601
:
Spherulites in in poly-3-hydroxy butyrate (PHB) System: Polyhydroxybutyrate (PHB), Composition: Not specified Cross-polarised light microscopy 240 nm |
![]() |
Micrograph
646
:
Spherulite growth imaged by atomic force microscopy (AFM) System: Polyhydroxybutyrate (PHB), Composition: Not specified Atomic force microscopy (AFM) 500 nm |
![]() |
Micrograph
647
:
A spherulite imaged by atomic force microscopy (AFM) System: Polyhydroxybutyrate (PHB), Composition: Not specified Atomic force microscopy (AFM) 3 μm |
![]() |
Micrograph
648
:
A spherulite imaged by atomic force microscopy (AFM) System: Polyhydroxybutyrate (PHB), Composition: Not specified Atomic force microscopy (AFM) 2 μm |