System
13 micrographs for system CCcomposite, ordered by micrograph number.
Showing 11 - 13 of 13 micrographs | Page 1 2 | Previous | Next |
Micrograph
672
:
Carbon-carbon composite System: CCcomposite, Composition: Not specified Reflected light microscopy 100 μm |
|
Micrograph
673
:
Carbon-carbon composite System: CCcomposite, Composition: Not specified Reflected light microscopy 50 μm |
|
Micrograph
674
:
Carbon-carbon composite System: CCcomposite, Composition: Not specified Reflected light microscopy 20 μm |
Showing 11 - 13 of 13 micrographs | Page 1 2 | Previous | Next |