564 micrographs for technique Reflected light microscopy, ordered by micrograph number.
Showing 101 - 110 of 564 micrographs | Page 1 .. 8 9 10 11 12 13 14 .. 57 | Previous | Next |
Micrograph
206
:
Normalised low carbon manganese steel, taken transverse to directionality System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
207
:
Normalised low carbon manganese steel, taken transverse to directionality System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
208
:
Normalised low carbon manganese steel, taken transverse to directionality System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
209
:
As cast carbon steel System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
210
:
As cast carbon steel System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
211
:
Normalised carbon steel System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
212
:
Normalised carbon steel System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
213
:
Normalised carbon steel System: Fe-C-X, Composition: Fe, C 0.15 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
214
:
Normalised carbon steel System: Fe-C-X, Composition: Fe, C 0.15 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
215
:
Normalised carbon steel System: Fe-C-X, Composition: Fe, C 0.08 (wt%) Reflected light microscopy 400 μm |
Showing 101 - 110 of 564 micrographs | Page 1 .. 8 9 10 11 12 13 14 .. 57 | Previous | Next |