793
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
794
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 20 μm |
|
Micrograph
795
:
Blackheart cast iron System: Fe-C-X, Composition: Blackheart cast iron Reflected light microscopy 100 μm |
|
Micrograph
796
:
Blackheart cast iron System: Fe-C-X, Composition: Blackheart cast iron Reflected light microscopy 100 μm |
|
Micrograph
797
:
Wear-resistant high-chromium cast iron System: Fe-C-X, Composition: Fe, C 2.6, Cr 17, Mo 2, Ni 2 (wt%) Reflected light microscopy 40 μm |
|
Micrograph
798
:
Wear-resistant high-chromium cast iron System: Fe-C-X, Composition: Fe, C 2.6, Cr 17, Mo 2, Ni 2 (wt%) Reflected light microscopy 20 μm |
|
Micrograph
802
:
Austenitic stainless steel solution treated, water quenched then tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Reflected light microscopy 50 μm |
|
Micrograph
806
:
Austenitic stainless steel water quenched then cooled, showing transformation to g in the a lamellae System: Fe-C-X, Composition: Fe, C 0.12, Mn 14.2, Cr 13.7 Reflected light microscopy 50 μm |
|
Micrograph
819
:
Austenitic stainless steel water quenched then deformed in impact System: Fe-C-X, Composition: Stainless steel with Cr 13.7, Mn 14.2, C 0.12 (wt%) Reflected light microscopy 50 μm |
|
Micrograph
833
:
Austenitic stainless steel solution treated, quenched then tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Reflected light microscopy 50 μm |