564 micrographs for technique Reflected light microscopy, ordered by micrograph number.
Showing 551 - 560 of 564 micrographs | Page 1 .. 51 52 53 54 55 56 57 | Previous | Next |
Micrograph
942
:
Kupferberg, Fichtel mountain, Germany. Speiss from copper production System: Cu production, Composition: Not specified Reflected light microscopy 500 μm |
|
Micrograph
943
:
Lead tube, recent System: Pb, Composition: Not specified Reflected light microscopy 500 μm |
|
Micrograph
944
:
Monte Romero, Huelva district, Spain. Phoenician, preroman silverproduction from complex ores. System: Pre-Roman Ag production, Composition: Not specified Reflected light microscopy 200 μm |
|
Micrograph
948
:
Experimental hammerscale, Denig, Kaiserslautern, Germany System: Smithing slag, Composition: Not specified Reflected light microscopy 100 μm |
|
Micrograph
953
:
Afunfun, Niger. Melilith-pyroxene-slag System: Cu production, Composition: Not specified Reflected light microscopy 200 μm |
|
Micrograph
954
:
Afunfun, Niger. Melilith-pyroxene-copper slag System: Cu production, Composition: Not specified Reflected light microscopy 200 μm |
|
Micrograph
955
:
Afunfun, Niger. Melilith-pyroxene-copper slag System: Cu production, Composition: Not specified Reflected light microscopy 100 μm |
|
Micrograph
956
:
Carthage, smithing slag, phoenician System: Smithing slag, Composition: Not specified Reflected light microscopy 500 μm |
|
Micrograph
957
:
Kupferberg, Fichtel mountain, Germany. Speiss from copper production System: Cu production, Composition: Not specified Reflected light microscopy 200 μm |
|
Micrograph
958
:
Kupferberg, Fichtel mountain, Germany. Speiss from copper production System: Cu production, Composition: Not specified Reflected light microscopy 100 μm |