Technique
87 micrographs for technique Scanning electron microscopy (SEM), ordered by micrograph number.
Showing 11 - 20 of 87 micrographs | Page 1 2 3 4 5 6 7 .. 9 | Previous | Next |
Micrograph
78
:
Forging steel, brittle, intergranular fracture System: Fe-C-X, Composition: Forging steel Scanning electron microscopy (SEM) 800 μm |
|
Micrograph
79
:
Ni-superalloy, fatigue crack propagation System: Ni-X, Composition: Not specified (Ni-Superalloy) Scanning electron microscopy (SEM) 150 μm |
|
Micrograph
80
:
Ni-superalloy, fatigue crack propagation System: Ni-X, Composition: Not specified (Ni-Superalloy) Scanning electron microscopy (SEM) 80 μm |
|
Micrograph
81
:
Ni-superalloy, fatigue crack propagation System: Ni-X, Composition: Not specified (Ni-Superalloy) Scanning electron microscopy (SEM) 30 μm |
|
Micrograph
82
:
Aluminium, fracture surface System: Al, Composition: Not specified Scanning electron microscopy (SEM) 15 μm |
|
Micrograph
83
:
Aluminium, fracture surface System: Al, Composition: Not specified Scanning electron microscopy (SEM) 50 μm |
|
Micrograph
114
:
Poly (lactic-co-glycolic acid) (PLGA) porous scaffold for tissue engineering. Average Pore Size 350-550 micrometre, porosity estimated at 35-45% System: Poly (lactic-co-glycolic acid) (PLGA), Composition: Not specified Scanning electron microscopy (SEM) 3 mm |
|
Micrograph
115
:
Poly (lactic-co-glycolic acid) (PLGA) porous scaffold for tissue engineering. Average Pore Size 350-550 micrometre, porosity estimated at 35-45% System: Poly (lactic-co-glycolic acid) (PLGA), Composition: Not specified Scanning electron microscopy (SEM) 250 μm |
|
Micrograph
116
:
Poly (lactic-co-glycolic acid) (PLGA) porous scaffold for tissue engineering. Enlargement of a Pore. Average Pore Size 350-550 mm, porosity estimated at 35-45% System: Poly (lactic-co-glycolic acid) (PLGA), Composition: Not specified Scanning electron microscopy (SEM) 250 μm |
|
Micrograph
117
:
Sintered disc of Hydroxyapatite (Ca10(PO4)6(OH)2), a calcium phosphate ceramic with similar composition to natural bone mineral System: Hydroxyapatite (Ca10(PO4)6(OH)2), Composition: Not specified Scanning electron microscopy (SEM) 18 μm |
Showing 11 - 20 of 87 micrographs | Page 1 2 3 4 5 6 7 .. 9 | Previous | Next |