Micrograph
969
:
Copper slag Wadi Arabah, Negev, Israel System: Cu production, Composition: Not specified Transmitted light microscopy 200 μm |
|
Micrograph
971
:
Sierra de Gador, Almeria, Spain. Subrecent lead slag System: Pb, Composition: Not specified Transmitted light microscopy 1 mm |
|
Micrograph
972
:
Smithing slag Carthage, phoenician System: Smithing slag, Composition: Not specified Transmitted light microscopy 200 μm |
|
Micrograph
973
:
Dasht-e-Kavir, Saghand, Central Iran. Lead slag System: Pb, Composition: Not specified Transmitted light microscopy 500 μm |
|
Micrograph
974
:
Dasht-e-Kavir, Saghand - Posht-e-Badam. Copper slag System: Cu production, Composition: Not specified Transmitted light microscopy 200 μm |
|
Micrograph
975
:
Dasht-e-Kavir, Saghand - Posht-e-Badam. Copper slag System: Cu production, Composition: Not specified Transmitted light microscopy 200 μm |