Partial pressure of oxidation: additional information
This can be explained in several ways.
At equilibrium, the total free energy of the each compound in the vapour phase must be equal to the total free energy of it in the solid phase. The free energy of the metal and the metal oxide in vapour form is very much greater than when in the solid form. This means that the amount of each in the vapour phase is very small and, as it turns out, negligible.
Secondly, a more general form of the equilibrium constant can be found. We derived it as above using the equation of state for an ideal gas-a specific case. Derived in another way (from the law of mass action) the equilibrium constant has the form
\[K = \frac{{{a_C}}}{{{a_A}{a_B}}}\]where ai is the activity of the ith component of the system. The activity of a component is its ability to take part in a reaction, and is directly related to the quantity of the component compared with its standard state, be it a gas, a pure solid, or the component of a solution.
In this case, since the metal and the oxide that are formed are assumed to be pure solids, they are already in their standard state, and their activity is therefore 1. The standard state of a gas is often (as it was above) defined as 1 bar. We hence find our equilibrium constant to be
\[K = \frac{{{a_C}}}{{{a_A}{a_B}}} = \frac{1}{{1p_{{O_2}}^{1/2}}}\]