Categories > Metal or alloy > Fe, C 0.4, Ni 1.3, Cr 0.65, Mo 0.65 (wt%)
5 micrographs available, ordered by micrograph number.
![]() |
Micrograph
326
:
Low alloy medium carbon steel, isothermally transformed System: Fe-C-X, Composition: Fe, C 0.4, Ni 1.3, Cr 0.65, Mo 0.65 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
327
:
Low alloy medium carbon steel, isothermally transformed System: Fe-C-X, Composition: Fe, C 0.4, Ni 1.3, Cr 0.65, Mo 0.65 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
345
:
Medium carbon, low alloy steel, isothermally transformed System: Fe-C-X, Composition: Fe, C 0.4, Ni 1.3, Cr 0.65, Mo 0.65 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
935
:
Dasht-e-Kavir, Saghand - Posht-e-Badam. Copper slag System: Fe-C-X, Composition: Fe, C 0.4, Ni 1.3, Cr 0.65, Mo 0.65 (wt%) Reflected light microscopy 2 mm |
![]() |
Micrograph
936
:
Shirnu Central Iran. Copper production slag System: Fe-C-X, Composition: Fe, C 0.4, Ni 1.3, Cr 0.65, Mo 0.65 (wt%) Transmitted light microscopy 1 mm |