Full Record for Micrograph 935
- Micrograph no
- 935
- Brief description
- Dasht-e-Kavir, Saghand - Posht-e-Badam. Copper slag
- Keywords
- Categories
- Metal or alloy
- System
- Fe-C-X
- Composition
- Fe, C 0.4, Ni 1.3, Cr 0.65, Mo 0.65 (wt%)
- Standard codes
- BS 640M40, formerly En 111
- Reaction
- Processing
- Applications
- Sample preparation
- Thin slide, double sided polished. 30-40 µm
- Technique
- Reflected light microscopy
- Length bar
- 2 mm
- Further information
- Contributor
- Dr Ingo Keesmann
- Organisation
- Johannes Gutenberg-Universitat Mainz
- Date
- 15/10/10
- Licence for re-use