Categories > Metal or alloy > Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%) > Reflected light microscopy > Keyword: alloy

5 micrographs available, ordered by micrograph number.


Link to full record for micrograph 420 Micrograph 420 : Commercial brass, ~30% Zn, displaying dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 421 Micrograph 421 : Commercial brass, ~30% Zn, displaying dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 422 Micrograph 422 : Commercial brass, ~30% Zn, displaying dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 423 Micrograph 423 : Commercial brass, ~30% Zn, displaying dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 424 Micrograph 424 : Commercial brass, ~30% Zn, displaying dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%)
Reflected light microscopy
200 μm