Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Browse the Library
Categories > Metal or alloy > Bi 80, Sn 20 (wt%)
4 micrographs available, ordered by micrograph number.
![]() |
Micrograph
765
:
Bi 80, Sn 20 (wt%) System: Bi-Sn, Composition: Bi 80, Sn 20 (wt%) Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode 300 μm |
![]() |
Micrograph
766
:
Bi 80, Sn 20 (wt%) System: Bi-Sn, Composition: Bi 80, Sn 20 (wt%) Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode 100 μm |
![]() |
Micrograph
767
:
Bi 80, Sn 20 (wt%) System: Bi-Sn, Composition: Bi 80, Sn 20 (wt%) Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode 10 μm |
![]() |
Micrograph
860
:
Bi 80wt%, Sn 20wt% System: Bi-Sn, Composition: Bi 80, Sn 20 (wt%) Reflected light microscopy 100 μm |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.