Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Full Record for Micrograph 860
- Micrograph no
- 860
- Brief description
- Bi 80wt%, Sn 20wt%
- Keywords
- Categories
- Metal or alloy
- System
- Bi-Sn
- Composition
- Bi 80, Sn 20 (wt%)
- Standard codes
- Reaction
- Processing
- Applications
- Sample preparation
- Technique
- Reflected light microscopy
- Length bar
- 100 μm
- Further information
- A hypereutectic (in wt% Bi) Bi-Sn alloy.
- Contributor
- Lewis Lea
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 12/08/10
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International- Related micrographs