Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Browse the Library
Categories > Metal or alloy > Stainless steel with Cr 15, Ni 35, Mo 2.5, C 0.25 (wt%)
1 micrograph available, ordered by micrograph number.
![]() |
Micrograph
804
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, Mo 2.5, C 0.25 (wt%) Scanning electron microscopy (SEM) 4 μm |