Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Full Record for Micrograph 804
- Micrograph no
- 804
- Brief description
- Austenitic stainless steel tempered
- Keywords
- austenite
, stainless steel - Categories
- Metal or alloy
- System
- Fe-C-X
- Composition
- Stainless steel with Cr 15, Ni 35, Mo 2.5, C 0.25 (wt%)
- Standard codes
- Reaction
- Processing
- Tempered 1000 hours at 700ºC
- Applications
- Sample preparation
- Carbon extraction replica
- Technique
- Scanning electron microscopy (SEM)
- Length bar
- 4 μm
- Further information
- Contributor
- Professor Sir R W K Honeycombe
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 07/01/04
- Licence for re-use
DoITPoMS standard terms of use