Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Contributor
36 micrographs contributed by Professor Sir R W K Honeycombe, ordered by micrograph number.
| Showing 1 - 10 of 36 micrographs | Page 1 2 3 4 | Previous | Next |
![]() |
Micrograph
799
:
Austenitic stainless steel solution treated, water quenched and tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Scanning electron microscopy (SEM) 2 μm |
![]() |
Micrograph
800
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Nb 1 (wt%) Scanning electron microscopy (SEM) 1 μm |
![]() |
Micrograph
801
:
Austenitic stainless steel solution treated, water quenched then tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Transmission electron microscopy (TEM) 400 nm |
![]() |
Micrograph
802
:
Austenitic stainless steel solution treated, water quenched then tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Reflected light microscopy 50 μm |
![]() |
Micrograph
803
:
Austenitic stainless steel solution treated, water quenched then tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Transmission electron microscopy (TEM) 1 μm |
![]() |
Micrograph
804
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, Mo 2.5, C 0.25 (wt%) Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
805
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, V 5, C 0.1 (wt%) Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
806
:
Austenitic stainless steel water quenched then cooled, showing transformation to g in the a lamellae System: Fe-C-X, Composition: Fe, C 0.12, Mn 14.2, Cr 13.7 Reflected light microscopy 50 μm |
![]() |
Micrograph
807
:
Martensitic steel solution treated and rapidly cooled with dislocation in retained autenite System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 500 nm |
![]() |
Micrograph
808
:
Martensitic steel tempered with precipitation of Mo2C System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 200 nm |
| Showing 1 - 10 of 36 micrographs | Page 1 2 3 4 | Previous | Next |