Categories > Metal or alloy > Fe, C 1, Mn 2, Si 1.5, Cr 1.3 (wt%)
2 micrographs available, ordered by micrograph number.
![]() |
Micrograph
134
:
High carbon steel System: Fe-C-X, Composition: Fe, C 1, Mn 2, Si 1.5, Cr 1.3 (wt%) Transmission electron microscopy (TEM) 600 nm |
![]() |
Micrograph
135
:
High carbon steel System: Fe-C-X, Composition: Fe, C 1, Mn 2, Si 1.5, Cr 1.3 (wt%) Transmission electron microscopy (TEM) 1.5 μm |