Micrograph
133
:
Steel, austenitised at 1200 centigrade for 120 s and then transformed isothermally at 350 centigrade for 2000 s before cooling to room temperature. System: Fe-C-X, Composition: Fe, C 0.24, Si 2.18, Mn 2.32, Ni 1.05 (wt%) Atomic force microscopy (AFM) 1 μm |
![]() |
Micrograph
134
:
High carbon steel System: Fe-C-X, Composition: Fe, C 1, Mn 2, Si 1.5, Cr 1.3 (wt%) Transmission electron microscopy (TEM) 600 nm |
![]() |
Micrograph
135
:
High carbon steel System: Fe-C-X, Composition: Fe, C 1, Mn 2, Si 1.5, Cr 1.3 (wt%) Transmission electron microscopy (TEM) 1.5 μm |
![]() |
Micrograph
311
:
Fe, C 0.4 (wt%) steel, slow quenched System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
312
:
Fe, C 0.4 (wt%) steel, slow quenched System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
739
:
TRIP steel annealed at 775°C for 5 mins and then hold at 400°C for 150s for austenite stabilization System: Fe-C-X, Composition: Fe, C 0.15, Mn 1.5, Si 1.5 (wt%) Reflected light microscopy 6 μm |
![]() |
Micrograph
740
:
TRIP steel annealed at 775°C for 5 mins and then hold at 400°C for 40s for austenite stabilization System: Fe-C-X, Composition: Fe, C 0.15, Mn 1.5, Si 1.5 (wt%) Reflected light microscopy 20 μm |