67
:
Hypoeutectic white cast iron System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 80 μm |
|
Micrograph
70
:
Silal System: Fe-C-X, Composition: Fe, C 3.0, Si 6, Mn 0.7, P 0.3, S 0.1 (wt% typical) (Silal) Reflected light microscopy 200 μm |
|
Micrograph
71
:
Silal System: Fe-C-X, Composition: Fe, C 3.0, Si 6, Mn 0.7, P 0.3, S 0.1 (wt% typical) (Silal) Reflected light microscopy 80 μm |
|
Micrograph
72
:
Ni-hard iron System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron) Reflected light microscopy 400 μm |
|
Micrograph
73
:
Ni-hard iron System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron) Reflected light microscopy 80 μm |
|
Micrograph
420
:
Commercial brass, ~30% Zn, displaying dendritic solidification System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
421
:
Commercial brass, ~30% Zn, displaying dendritic solidification System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
422
:
Commercial brass, ~30% Zn, displaying dendritic solidification System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
423
:
Commercial brass, ~30% Zn, displaying dendritic solidification System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
424
:
Commercial brass, ~30% Zn, displaying dendritic solidification System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%) Reflected light microscopy 200 μm |
Showing 11 - 20 of 77 micrographs | Page 1 2 3 4 5 6 7 8 | Previous | Next |