Categories > Metal or alloy > Keyword: normalising

29 micrographs available, ordered by micrograph number.


Showing 1 - 10 of 29 micrographs Page 1 2 3 | Previous | Next

Link to full record for micrograph 201 Micrograph 201 : Normalised low carbon steel, showing directionality
System: Fe-C-X, Composition: Wrought iron (plain carbon steel)
Reflected light microscopy
400 μm
Link to full record for micrograph 202 Micrograph 202 : Normalised low carbon steel, showing directionality
System: Fe-C-X, Composition: Wrought iron (plain carbon steel)
Reflected light microscopy
200 μm
Link to full record for micrograph 203 Micrograph 203 : Normalised low carbon manganese steel, showing directionality
System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 204 Micrograph 204 : Normalised low carbon manganese steel, showing directionality
System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 205 Micrograph 205 : Normalised low carbon manganese steel, taken transverse to directionality
System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 206 Micrograph 206 : Normalised low carbon manganese steel, taken transverse to directionality
System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 211 Micrograph 211 : Normalised carbon steel
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 245 Micrograph 245 : Fe, C 1.3 (wt%) steel, normalised at 1050°C
System: Fe-C-X, Composition: Fe, C 1.3 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 246 Micrograph 246 : Fe, C 1.3 (wt%) steel, normalised at 1050°C
System: Fe-C-X, Composition: Fe, C 1.3 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 247 Micrograph 247 : Fe, C 1.3 (wt%) steel, normalised at 1050°C
System: Fe-C-X, Composition: Fe, C 1.3 (wt%)
Reflected light microscopy
100 μm