Full Record for Micrograph 205
[184 KB]
View micrograph
.. in new window
View micrograph and record
.. in new window
You can also view and download the micrographs on Flickr
- Micrograph no
- 205
- Brief description
- Normalised low carbon manganese steel, taken transverse to directionality
- Keywords
- alloy
, carbon, directionality, iron, metal, normalising
, steel 
- Categories
- Metal or alloy
- System
- Fe-C-X
- Composition
- Fe, C 0.1, Mn 1, S 0.5 (wt%)
- Standard codes
- Reaction
- Processing
- Hot worked normalised 1000 ºC
- Applications
- Sample preparation
- Nital
- Technique
- Reflected light microscopy
- Length bar
- 400 μm
- Further information
- Low carbon steel with a microstructure consisting mostly of ferrite. Manganese is added to steel to remove oxygen and sulphur. It causes a reduction in the resulting grain size and hence the steel is tougher and stronger. This sample has been normalised, recrystallising the ferrite. This micrograph has been taken transverse to the directionality and hence the directionality present in the pearlite is not apparent
- Contributor
- Dr R F Cochrane
- Organisation
- Department of Materials, University of Leeds
- Date
- 04/09/02
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International- Related micrographs