Keyword
6 micrographs for keyword directionality, ordered by micrograph number.
![]() |
Micrograph
201
:
Normalised low carbon steel, showing directionality System: Fe-C-X, Composition: Wrought iron (plain carbon steel) Reflected light microscopy 400 μm |
![]() |
Micrograph
202
:
Normalised low carbon steel, showing directionality System: Fe-C-X, Composition: Wrought iron (plain carbon steel) Reflected light microscopy 200 μm |
![]() |
Micrograph
203
:
Normalised low carbon manganese steel, showing directionality System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
204
:
Normalised low carbon manganese steel, showing directionality System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
205
:
Normalised low carbon manganese steel, taken transverse to directionality System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
206
:
Normalised low carbon manganese steel, taken transverse to directionality System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%) Reflected light microscopy 200 μm |