Browse the Library
Categories > Metal or alloy > Keyword: recrystallisation
17 micrographs available, ordered by micrograph number.
Showing 1 - 10 of 17 micrographs | Page 1 2 | Previous | Next |
Micrograph
31
:
Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
32
:
Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 40 μm |
|
Micrograph
33
:
Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
34
:
Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
35
:
Cu 70, Zn 30 (wt%), faster recrystallisation - finer grain size System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
37
:
Cu 70, Zn 30 (wt%), slow cooling - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
38
:
Cu 98, Be 2 (wt%), slow cooling - annealing twins System: Cu-Be, Composition: Cu 98, Be 2 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
156
:
Roll-bonded aluminium alloy diffusion couple annealed for 30 minutes at 600ºC. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 400 μm |
|
Micrograph
157
:
Roll-bonded aluminium alloy diffusion couple annealed for 60 minutes at 600ºC. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 750 μm |
|
Micrograph
211
:
Normalised carbon steel System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 400 μm |
Showing 1 - 10 of 17 micrographs | Page 1 2 | Previous | Next |