Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Browse the Library
Categories > Metal or alloy > Keyword: brass
67 micrographs available, ordered by micrograph number.
| Showing 1 - 10 of 67 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |
![]() |
Micrograph
29
:
Cu 70, Zn 30 (wt%), annealed and cold rolled System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
30
:
Cu 70, Zn 30 (wt%), annealed and cold rolled System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 40 μm |
![]() |
Micrograph
31
:
Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
32
:
Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 40 μm |
![]() |
Micrograph
33
:
Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
34
:
Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
35
:
Cu 70, Zn 30 (wt%), faster recrystallisation - finer grain size System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
36
:
Cu 60, Zn 40 (wt%), quenched - metastable b grains System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
37
:
Cu 70, Zn 30 (wt%), slow cooling - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
49
:
Cu 60, Zn 40 (wt%), slow cooling - equiaxed grains System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 400 μm |
| Showing 1 - 10 of 67 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.