Micrograph
140
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
|
Micrograph
141
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
|
Micrograph
142
:
Tough pitch copper, failed by fibrous ductile fracture. System: Cu, Composition: Tough pitch copper Scanning electron microscopy (SEM) 20 μm |
|
Micrograph
156
:
Roll-bonded aluminium alloy diffusion couple annealed for 30 minutes at 600ºC. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 400 μm |
|
Micrograph
157
:
Roll-bonded aluminium alloy diffusion couple annealed for 60 minutes at 600ºC. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 750 μm |
|
Micrograph
158
:
Roll-bonded aluminium alloy diffusion couple in the as-rolled condition. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 400 μm |
|
Micrograph
159
:
Roll-bonded aluminium alloy diffusion couple in the as-rolled condition. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 2 mm |
|
Micrograph
604
:
Extruded aluminium System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy, polarised 40 μm |
|
Micrograph
608
:
Channelling contrast TEM image of subgrains of extruded aluminium System: Al, Composition: Commercial purity (99.5%) Transmission electron microscopy (TEM) 600 nm |
|
Micrograph
609
:
The grain structure of extruded aluminium System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy, polarised 40 μm |