Browse the Library
Categories > Metal or alloy > Keyword: aluminium
60 micrographs available, ordered by micrograph number.
Showing 31 - 40 of 60 micrographs | Page 1 2 3 4 5 6 | Previous | Next |
Micrograph
613
:
Facetted aluminium dendrites System: Al-Sn, Composition: Al 15, Sn 85 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
615
:
Cross-section of an aluminium casting System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy 10 mm |
|
Micrograph
629
:
FORMGRIP closed cell aluminium foam System: Al, Composition: Not specified Photography (no microscope) 6 mm |
|
Micrograph
630
:
FOAMCARP closed cell aluminium foam System: Al, Composition: Not specified Photography (no microscope) 6 mm |
|
Micrograph
631
:
Coarse open celled aluminium foam produced by infiltration of sintered salt (FOAM-U-LIKE) System: Al, Composition: Not specified Photography (no microscope) 6 mm |
|
Micrograph
632
:
Open-celled aluminium foam System: Al, Composition: Not specified Photography (no microscope) 8 mm |
|
Micrograph
633
:
Cross-section of an aluminium foam slab produced by gas injection System: Al, Composition: Not specified Photography (no microscope) 10 mm |
|
Micrograph
634
:
Solid-gas eutectic solidification (Gasar) aluminium foam System: Al, Composition: Not specified Photography (no microscope) 120 μm |
|
Micrograph
635
:
Open celled aluminium foam produced by infiltration of sintered salt System: Al, Composition: Not specified Scanning electron microscopy (SEM) 400 μm |
|
Micrograph
636
:
Alporas' closed cell aluminium foam System: Al, Composition: Not specified Photography (no microscope) 6 mm |
Showing 31 - 40 of 60 micrographs | Page 1 2 3 4 5 6 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.