Link to full record for micrograph 135 Micrograph 135 : High carbon steel
System: Fe-C-X, Composition: Fe, C 1, Mn 2, Si 1.5, Cr 1.3 (wt%)
Transmission electron microscopy (TEM)
1.5 μm
Link to full record for micrograph 143 Micrograph 143 : Notched low carbon ferritic steel, failed through cleavage.
System: Fe-C-X, Composition: Not specified
Scanning electron microscopy (SEM)
20 μm
Link to full record for micrograph 146 Micrograph 146 : HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture.
System: Fe-C-X, Composition: Not specified
Scanning electron microscopy (SEM)
200 μm
Link to full record for micrograph 147 Micrograph 147 : HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture.
System: Fe-C-X, Composition: Not specified
Scanning electron microscopy (SEM)
200 μm
Link to full record for micrograph 201 Micrograph 201 : Normalised low carbon steel, showing directionality
System: Fe-C-X, Composition: Wrought iron (plain carbon steel)
Reflected light microscopy
400 μm
Link to full record for micrograph 202 Micrograph 202 : Normalised low carbon steel, showing directionality
System: Fe-C-X, Composition: Wrought iron (plain carbon steel)
Reflected light microscopy
200 μm
Link to full record for micrograph 203 Micrograph 203 : Normalised low carbon manganese steel, showing directionality
System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 204 Micrograph 204 : Normalised low carbon manganese steel, showing directionality
System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 205 Micrograph 205 : Normalised low carbon manganese steel, taken transverse to directionality
System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 206 Micrograph 206 : Normalised low carbon manganese steel, taken transverse to directionality
System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%)
Reflected light microscopy
200 μm

Showing 21 - 30 of 172 micrographs Page 1 2 3 4 5 6 7 .. 18 | Previous | Next

Help is available on browsing.

Alternatively, search the Library (from top right on any page), or use advanced search.