Browse the Library
Categories > Metal or alloy
708 micrographs available, ordered by micrograph number.
| Showing 91 - 100 of 708 micrographs | Page 1 .. 7 8 9 10 11 12 13 .. 71 | Previous | Next |
![]() |
Micrograph
143
:
Notched low carbon ferritic steel, failed through cleavage. System: Fe-C-X, Composition: Not specified Scanning electron microscopy (SEM) 20 μm |
![]() |
Micrograph
144
:
Zinc, notched specimen, failed through brittle cleavage fracture. System: Zn, Composition: Not specified Scanning electron microscopy (SEM) 200 μm |
![]() |
Micrograph
145
:
Zinc, notched specimen, failed through brittle cleavage fracture. System: Zn, Composition: Not specified Scanning electron microscopy (SEM) 1 mm |
![]() |
Micrograph
146
:
HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture. System: Fe-C-X, Composition: Not specified Scanning electron microscopy (SEM) 200 μm |
![]() |
Micrograph
147
:
HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture. System: Fe-C-X, Composition: Not specified Scanning electron microscopy (SEM) 200 μm |
![]() |
Micrograph
156
:
Roll-bonded aluminium alloy diffusion couple annealed for 30 minutes at 600ºC. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 400 μm |
![]() |
Micrograph
157
:
Roll-bonded aluminium alloy diffusion couple annealed for 60 minutes at 600ºC. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 750 μm |
![]() |
Micrograph
158
:
Roll-bonded aluminium alloy diffusion couple in the as-rolled condition. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 400 μm |
![]() |
Micrograph
159
:
Roll-bonded aluminium alloy diffusion couple in the as-rolled condition. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 2 mm |
![]() |
Micrograph
201
:
Normalised low carbon steel, showing directionality System: Fe-C-X, Composition: Wrought iron (plain carbon steel) Reflected light microscopy 400 μm |
| Showing 91 - 100 of 708 micrographs | Page 1 .. 7 8 9 10 11 12 13 .. 71 | Previous | Next |