Categories > Metal or alloy

708 micrographs available, ordered by micrograph number.


Showing 301 - 310 of 708 micrographs Page 1 .. 28 29 30 31 32 33 34 .. 71 | Previous | Next

Link to full record for micrograph 412 Micrograph 412 : Cast iron, containing phosphorus
System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 413 Micrograph 413 : Cast iron, containing phosphorus
System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 414 Micrograph 414 : Cast iron, containing phosphorus
System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 415 Micrograph 415 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
800 μm
Link to full record for micrograph 416 Micrograph 416 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
200 μm
Link to full record for micrograph 417 Micrograph 417 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy, polarised with wave-plate
800 μm
Link to full record for micrograph 418 Micrograph 418 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
400 μm
Link to full record for micrograph 419 Micrograph 419 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
100 μm
Link to full record for micrograph 420 Micrograph 420 : Commercial brass, ~30% Zn, displaying dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 421 Micrograph 421 : Commercial brass, ~30% Zn, displaying dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%)
Reflected light microscopy
400 μm

Showing 301 - 310 of 708 micrographs Page 1 .. 28 29 30 31 32 33 34 .. 71 | Previous | Next