Browse the Library
Categories > Metal or alloy
708 micrographs available, ordered by micrograph number.
| Showing 661 - 670 of 708 micrographs | Page 1 .. 64 65 66 67 68 69 70 71 | Previous | Next |
![]() |
Micrograph
928
:
Edo time japanese sword System: Ti-Al-V, Composition: Ti, Al 6, V 4 (wt%) Reflected light microscopy 2 mm |
![]() |
Micrograph
929
:
Edo time japanese sword System: Ti-Al-V, Composition: Ti, Al 6, V 4 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
930
:
Manching oppidum, Ingolstadt, Germany System: Cu production, Composition: Not specified Transmitted light microscopy 500 μm |
![]() |
Micrograph
931
:
Afunfun, Niger. Melilith-pyroxene-copper slag System: Cu production, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
932
:
Nörten-Hardenberg (Goettingen) Germany. Smithing slag (hallstatt - latène) System: Smithing slag, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
933
:
Dasht-e-Kavir, Saghand - Posht-e-Badam. Copper slag System: Cu production, Composition: Not specified Transmitted light microscopy 500 μm |
![]() |
Micrograph
934
:
Experimental iron production, Ph. Andrieux, Paris System: Fe production, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
935
:
Dasht-e-Kavir, Saghand - Posht-e-Badam. Copper slag System: Fe-C-X, Composition: Fe, C 0.4, Ni 1.3, Cr 0.65, Mo 0.65 (wt%) Reflected light microscopy 2 mm |
![]() |
Micrograph
936
:
Shirnu Central Iran. Copper production slag System: Fe-C-X, Composition: Fe, C 0.4, Ni 1.3, Cr 0.65, Mo 0.65 (wt%) Transmitted light microscopy 1 mm |
![]() |
Micrograph
937
:
Fernando Lopez (Sierra Alhamilla), Almería, Spain System: Cu production, Composition: Not specified Reflected light microscopy 500 μm |
| Showing 661 - 670 of 708 micrographs | Page 1 .. 64 65 66 67 68 69 70 71 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.