Browse the Library
Categories > Metal or alloy > Al-Mg-Si
6 micrographs available, ordered by micrograph number.
![]() |
Micrograph
137
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
![]() |
Micrograph
138
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
![]() |
Micrograph
139
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
![]() |
Micrograph
140
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
![]() |
Micrograph
141
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
![]() |
Micrograph
843
:
Micrograph of base metal. T6 - solution heat treated and artificially aged. System: Al-Mg-Si, Composition: Al, Mg 1, Si 0.8, Mn 0.5 (wt%) Optical microscope, reflected light 250 μm |
Help is available on browsing.